Electron beam evaporation constitutes one of the most economic and widely used coating techniques. A major drawback, however, is the limited applicability to simple oxide and metal coatings. Novel concepts and e-beam sources allow extension of the application range to a lot of vacuum heating processes and deposition of complex compounds comprising constituents with widely differing volatility.