Dynamics Of Thermal Conditions Of Molds In Molding Glass Articles

It is proposed to introduce the concept of thermal stability in molds in the course of molding glass articles and a formula for calculating the stability coefficient, which will make it possible to model production conditions taking into account variations in the ambient temperature and molding duration.