The Dynamic Structure Of Glassy Materials

The structure of inorganic glasses is commonly shown as a modified random network in which the cations occupy interstitial sites. This model is good for silicate and for similar "polymeric" oxide glasses, in emphasising the distinctions between bridging and non-bridging oxygens and between the mobile cations and the immobile anionic framework. But is such a simple picture adequate to the needs of modern glass science? In particular, is it a valid starting point given the new spectroscopic data that are available? These questions can be briefly addressed in this paper.

Author
M D Ingram Et Al
Origin
University Of Aberdeen, Uk
Journal Title
Glastech Ber Glass Sci Technol 68 C1 1995 59-66
Sector
Special Glass
Class
S 1006

Request article (free for British Glass members)

The Dynamic Structure Of Glassy Materials
Glastech Ber Glass Sci Technol 68 C1 1995 59-66
S 1006
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.