Dust Control - Product Reclamation Or Legislative Necessity?

The need for more effective dust control equipment in industry, highlighted by the introduction of the COSHH regulations, is discussed with reference to the DCE Unimaster dust collector.

Author
J W Healey
Origin
Dce Ltd
Journal Title
Glass October 1989 412, 414