Durable Glass Ceramic Ferrule For General Telecommunication Use

Glass ceramic ferrules composed of Si02-Al203-Li20-Mg0-Ti02-Zr02-K20-Zn0-Ba0 have been fabricated by a preform drawing process. These ferrules show good durability in hot and humid conditions and when immersed in water. A glass ceramic ferrule is the most suitable ferrule to realise low cost optional connectors for fibre to the home.

Author
S Mitachi Et Al
Origin
Ntt Opto-Electronic Labs, Japan
Journal Title
Glass Technology 39 3 1998 98-99
Sector
Glass Ceramics
Class
GC 319

Request article (free for British Glass members)

Durable Glass Ceramic Ferrule For General Telecommunication Use
Glass Technology 39 3 1998 98-99
GC 319