Durability Of Glass Ceramic Jacketed Optical Fibre

A novel optical fibre connecting component was fabricated by direct jacketing of silica glass single mode optical fibre (SMF) with a low expansion Li2O-Al2O3-SiO2 (LAS) glass ceramic. The durability of the glass ceramic jacketed SMF (GC-SMF) was evaluated by immersion, high temperature and damp heat tests. The GC-SMF displayed excellent stability in the configuration of its optical connecting endfaces in both the immersion test in hot acidic water and the high temperature endurance test at 500 deg C for 1 hour. It was confirmed that the GC-SMF is suitable for high power optical communication systems as a durable optical connecting component.

Author
A Sakamoto Et Al
Origin
Nippon Electric Glass, Japan
Journal Title
Glass Technology 45 2 April 2004 84-87
Sector
Glass Ceramics
Class
GC 581

Request article (free for British Glass members)

Durability Of Glass Ceramic Jacketed Optical Fibre
Glass Technology 45 2 April 2004 84-87
GC 581
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.