Dta/Sem Study Of Crystallization In Sphene Glass-Ceramics

Differential thermal analysis and scanning electron microscopy have been used to study the nucleation and crystallisation during reheating of two titanosilicate glasses, the resulting sphene glass-ceramics being designed for the immobilisation of nuclear fuel recycle wastes.

Author
P J Hayward, E R Vance, D C Doern
Origin
Atomic Energy Of Canada Ltd.
Journal Title
Ceramic Bulletin 1987 66 11 1620-1626
Sector
Glass Ceramics
Class
GC 22