Dta, Density And Infrared Spectra Studies Of The Structure Of Vanadium Phosphate Glasses Containing Lithium Oxide

The effect of replacing V2O5 BY lI2o in vanadium phosphate glass was studied. Both infrared absorption spectra and differential thermal analysis, in addition to density measurements were performed. It was found that the number of oxygens increase in the network, also the vanadium ions are present in network forming positions, while lithium ions take only the interstitial positions.

Author
H Farouk Et Al
Origin
Azhar University, Egypt
Journal Title
Phys Chem Glasses 35 5 1994 207-209
Sector
Special Glass
Class
S 822

Request article (free for British Glass members)

Dta, Density And Infrared Spectra Studies Of The Structure Of Vanadium Phosphate Glasses Containing Lithium Oxide
Phys Chem Glasses 35 5 1994 207-209
S 822
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.