Dsc Thermal Anomalies In The Glass Transition Temperature Domain For A Boron Oxyfluoride (Bof) Glass

Heat capacity measurements by DSC in the glass transition domain of BO1.34Fo.32 glass have allowed the determination of two glass transition temperatures Tg on heating up to (Tg+80)K. This result is in good agreement with a previous structural characterisation of a BO1.32F0.36 glass by NMR, thus demonstrating the appearance of new polyhedral species near Tg and the formation of BF3 trapped in the glass matrix. The difference between the heat capacities of the solid and the liquid phases, 0.8J/gK, reveals the fragile character of the melt.

Author
M Matecki Et Al
Origin
Inst Science, France
Journal Title
Phys Chem Glasses 45 4 2004 223-226
Sector
Special Glass
Class
S 2868

Request article (free for British Glass members)

Dsc Thermal Anomalies In The Glass Transition Temperature Domain For A Boron Oxyfluoride (Bof) Glass
Phys Chem Glasses 45 4 2004 223-226
S 2868
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.