Drying Stages During The Heating Of High-Alumina, Ultra-Low-Cement Refractory Castables

The purpose of this work was to investigate the drying kinetics of high-alumina, ultra-low-cement refractory castables under continuous heating conditions. Three main drying stages were identified during the castable heat-up and were related to the phase change of free water and to the decomposition of hydrated products present in the body. A clear correlation was found between the actual heating profile inside the castable and the dewatering stages under various heating schedules. Thermal analysis was used to assess the drying temperature that represents the highest risk of steam pressure build-up and thus, of explosive spalling.

Author
M D M Innocentini
Origin
Federal University Of Sao Carlo, Brazil
Journal Title
Jacs 86 7 2003 1146-1148
Sector
Refractories
Class
R 499

Request article (free for British Glass members)

Drying Stages During The Heating Of High-Alumina, Ultra-Low-Cement Refractory Castables
Jacs 86 7 2003 1146-1148
R 499
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.