Drying And Curing Inks And Coatings On Glass

This article is the first of a two-part series on inks and coatings. The second article on how to troubleshoot common problems with inks will appear in the May 2013 issue. This particular issue concentrates on the types of inks and coatings that are available and how to properly dry and cure these - a process critical to creating high quality decoration on glass.

Author
D Canfield
Origin
Casso Solar, Usa
Journal Title
Glass Magazine April 2013 36-38
Sector
Enamels
Class
E 161