Dissolved Water

Hydrogen atoms are, on an atom-by-atom basis, the most influential constituents of oxide glasses. In the glass structure, these atoms reside in the form of hydroxyl ions bound to the glass-former cation, e.g. silicon, boron, germanium, of phosphorus. No other element has as great an effect on glass properties when concentrations are compared on an atomic basis. This effect is even more dramatic when properties are compared on a weight basis, since hydrogen is also the lightest of all elements. The effects of hydrogen ions, in the form of hydroxyl, on the properties and applications of glasses range from the depression of the viscosity to the enhancement of phase separation and crystallisation rates and to the absorption of light, which is so important for communication optical fibre technology.

Author
J E Shelby
Origin
Nys College Of Ceramics, Usa
Journal Title
The Glass Researcher 10Th Anniversary Collection 1986/96 17-18
Sector
Special Glass
Class
S 2578

Request article (free for British Glass members)

Dissolved Water
The Glass Researcher 10Th Anniversary Collection 1986/96 17-18
S 2578
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.