Dissolution Rates Of Commercial Soda-Lime And Pyrex Borosilicate Glasses: Influence Of Solution Ph

Dissolution rates of two commercial soda-lime silicate glasses and Pyrex borosilicate glass (Corning 7740) have been measured as a function of pH. The dissolution rate was constant with time and increased with increase in pH from 4 to 9.