Discharge Diagnosis And Controlled Deposition Of Snox:F Films By Dc-Reactive Sputtering From A Metallic Tin Target

Fluorine-doped tin oxide films on glass substrates have been prepared by reactive magnetron DC-sputtering in Ar-O2-Freon plasma from a metallic tin target. We studied the relationship between the discharge characteristics and film properties and found the discharge conditions in which the films belong tot he SnO2 or to the SnO stoichiometry, by proposing a phase diagram for this system. It was shown that the film stoichiometry is closely related to the tin valence changes at the target. We found that there is a narrow voltage band and a limit value in the oxygen content where the films have SnO2 stoichiometry; outside this region SnO films are obtained. We studied the crystallinity and the optical properties of the SnO2 films. The results show that crystalline films have cassiterite-like diffraction patterns with preferred orientation in the 100 planes.

Author
A Martel Et Al
Origin
University La Habana, Cuba
Journal Title
Surface & Coatings Technology 1999 122 136-142
Sector
Special Glass
Class
S 3020

Request article (free for British Glass members)

Discharge Diagnosis And Controlled Deposition Of Snox:F Films By Dc-Reactive Sputtering From A Metallic Tin Target
Surface & Coatings Technology 1999 122 136-142
S 3020
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.