Direct Joining Of Bscco Superconducting Glass-Ceramics Using A Flame-Melting Method

A new method for joining bismuth-based superconducting glass-ceramics has been developed; they are joined easily by melting-annealing with a liquid natural gas (LNG)-oxygen flame. Two edge portions of the glass-ceramics to be joined are melted by a high-temperature flame, and the molten faces are placed quickly against each other. Subsequently, the joined portion is annealed sufficiently with a soft flame, resulting in a unified product with no cracks. This technique is very important for fabrication of large-sized superconducting ceramics, such as bushing apparatuses.

Author
T Kasuga Et Al
Origin
Nagoya Inst Of Tech, Japan
Journal Title
J Am Ceram Soc 79 4 1996 885-888
Sector
Glass Ceramics
Class
GC 237

Request article (free for British Glass members)

Direct Joining Of Bscco Superconducting Glass-Ceramics Using A Flame-Melting Method
J Am Ceram Soc 79 4 1996 885-888
GC 237
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.