Direct-Flow Furnace For The Production Of Container Glass

Two container furnaces with pulls of 30 and 10 tonnes/day respectively are described. They are designed with a "thin-layer" refining zone (glass depth 150 mm) and are characterised by relatively low operating temperatures.