The "Direct Bond" In Magnesia Chromite And Magnesia Spinel Refractories

The microstructures of several commercial refractory bricks have been characterised using scanning and transmission electron microscopy. The "direct bond" is shown to be direct at the level of resolution attainable (~0.3nm), and a significant number of such direct contacts occur between non-silicate phases in the microstructures of magnesia-chromite bricks. However, attempts to examine the direct bond in magnesia-spinel bricks were unsuccessful due to nonuniform ion thinning of TEM specimens.

Author
K Goto & W E Lee
Origin
University Of Sheffield, Uk
Journal Title
J Am Ceram Soc 78 7 1995 1753-1760
Sector
Refractories
Class
R 172

Request article (free for British Glass members)

The "Direct Bond" In Magnesia Chromite And Magnesia Spinel Refractories
J Am Ceram Soc 78 7 1995 1753-1760
R 172
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.