Dimensionless Density: Packing And Structure In Oxide Glass Systems

Density is an essential comparative measure for all structural models of glasses. Molar volume and packing efficiency seek to normalise density for both the masses and volumes of ions before comparison to atomic-level order. In this presentation, packing fractions from five oxide glass systems were determined and compared to each other and to atomic-level structural models. Both short-range and intermediate-range order may be discerned in the resulting trends of packing fraction as a function of glass composition. Furthermore, in several specific glass systems, generalisations have been found in the packing trends that are independent of alkali type. In glasses with small modifier ions the packing is strongly influenced by the atomic structure of the glass forming network while in the case of larger modifiers random packaging of these large ions controls the overall packaging and is independent of modifier itself.

Author
S Feller
Origin
Coe College, Usa
Journal Title
13Th Symp Eu Soc Of Glass Science 2016 75
Sector
Special Glass
Class
S 4324

Request article (free for British Glass members)

Dimensionless Density: Packing And Structure In Oxide Glass Systems
13Th Symp Eu Soc Of Glass Science 2016 75
S 4324
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.