Digital Technologies For Automated Optical Sorting Of Recycled Glass

This article discusses the technology that is capable of recovering the three main colour fractions as well as removing ceramic and metal contaminants in one unit.

Author
F A Hottenstein & G R Kenny
Origin
Mss Inc, Usa
Journal Title
Glass 80 8 Sept/03 260