Digital Display: Measuring The Float Glass On The Prodcution Line

The Bendix Corporation has installed an automatic gauge in a Swedish float glass plant showing the thickness deviation from a nominally set point as well as the width of the glass ribbon and the drift from the secure centre line of the layer in a digital display.

Author
Anon
Origin
Unknown
Journal Title
American Glass Review 1976 96 (10) 9