Diffusion Of Water Into Silica Glass At Low Temperature

Diffusion of water into silica glass was measured in the temperature range 200-750 degrees C by treating the glass in air containing a constant water vapour pressure and analysing the concentration profile using a Fourier transform infrared spectrometer.