Differential Thermal Analysis On The Crystallization Kinetics Of K20-B203-Mg0-Al203-Si02-Ti02-F Glass

The crystallization kinetics of a glass based on one type of mica, NaMg3AlSi3010F2, with the addition of a nucleating agent, Ti02, has been studied using differential thermal analysis under both isothermal and nonisothermal conditions.