Dielectric Characteristics Of Silica Glasses And Their Relationship To Shg In Poled Silica

Electrical and dielectric relaxation measurements were conducted in silica glasses. Using the results of the measurements the cause of second harmonic generation (SHG) in thermally poled silica glass was considered. Absorption currents were measured as a function of time for various types of silica glasses and analysed using the theory of space charge polarisation. It was found that generation, annihilation, reproduction and temperature dependence of SHG in poled silica are similar to those of space charge polarisation.

Author
D W Shin & M Tomozawa
Origin
Hanyang University, Seoul, & Rensselaer Polytechnic, Usa
Journal Title
Phys Chem Glases 42 3 2001 199-206
Sector
Special Glass
Class
S 2284

Request article (free for British Glass members)

Dielectric Characteristics Of Silica Glasses And Their Relationship To Shg In Poled Silica
Phys Chem Glases 42 3 2001 199-206
S 2284
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.