The Dielectric Behaviour And Conduuction Of Agi-Agpo3 Glasses Of Various Compositions

The dialectric permittivity and loss of (AgI)x(AgPO3)1-x glasses for x = 0 to x = 0.7 in increments of 0.1 were measured from 12 Hz to 100 kHz in the temperature rate 77K to near their respective glass transition temperatures, in both their cooled and annealed states.