Devices For Monitoring Process Chemistry In Coated Float Glass

Efforts to develop microdevices for analyzing chemical content of complex mixtures of gases and liquids have increased over the last 10 years. Some devices are produced in miniature using advanced fabrication techniques, although they are based on the operating principles of traditional laboratory analytical instruments. Non-traditional devices that exploit electrochemical and/or catalytic properties of solids and interfaces take the form of analyte-specific solid state sensors. Performance of these devices rivals that of large-scale instruments. Their reduced size offers such advantages as ruggedness and decreased power consumption.

Author
A H Mcdaniel
Origin
Sandia Nat Labs, Usa
Journal Title
The Glass Researcher 10 1 2000 12-13, 20-21
Sector
Flat glass
Class
F 1166

Request article (free for British Glass members)

Devices For Monitoring Process Chemistry In Coated Float Glass
The Glass Researcher 10 1 2000 12-13, 20-21
F 1166
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.