Developments Of Siemens Regeerative And Tank Furnaces In Saint-Gobain In The 19Th Century

The developments in Siemens regenerative and tank furnaces in Saint-Gobain in the 19th century based on an analysis of data available in the Saint-Gobain archives are reviewed. The development of the relationship between William Siemens and Saint-Gobain is also covered.

Author
M Chopinet
Origin
Cnrs/Saint-Gobain, France
Journal Title
Glass Technol 53 5 2012 177-188