Developments In Low Emission Combustion

This paper discusses developments in Low NOx burning technology. The technique of the Multihole gas burner, patented by British Gas, has been applied to underport firing, throughport firing using water-cooled burners and burners for use on recuperative furnaces achieving remarkable NOx reduction.