Development Of Wall-Covering Glass-Ceramics From Raw Materials

The possibility of producing wall-covering glass-ceramic materials from raw materials by crystallisation of the glass is demonstrated. Glass-ceramics based on wollastonite and diopside with various ratios were designed from raw materials such as limestone and dolomite. The phases crystallised were examined by X-ray analysis. Thermal expansion and mechanical properties such as bending strength and microhardness for glasses and glass-ceramics were measured.

Author
S A M Abdel-Hameed
Origin
Nat Research Centre, Cairo
Journal Title
Glass Sci Technol 75 6 2002 290-293
Sector
Glass Ceramics
Class
GC 490

Request article (free for British Glass members)

Development Of Wall-Covering Glass-Ceramics From Raw Materials
Glass Sci Technol 75 6 2002 290-293
GC 490
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.