Development Of Translucent Glass-Ceramics For Dental Applications

The object of this study was to develop glass-ceramics with favourable properties for use in dentistry. This paper focuses on two glass-ceramic systems: SiO2-Al2O3-K2O-CaO-P2O5-F and SiO2-Li2O-ZrO2-P2O5. Phase development in the heat treated base glasses was primarily examined by scanning electron microscopy and X-ray diffraction.

Author
W Holand Et Al
Origin
Ivoclar Co Ltd, Principality Of Liechtenstein
Journal Title
5Th Int Otto Schott Colloquium, Jena, July 1994 117-122