Development Of A Technological Complex For Washing Sand

A technological complex was developed in order to remove clay minerals, iron oxide, and fractions heavier than 2.9 tons/m3 from glass quartz sands. The basis of the scheme of the apparatus chain of the complex consists of a trammel screen with a new design, jigs, and concentration tables with electromagnetic inductors. It was shown under laboratory conditions that sand in the highest demand — VS-030-V grade — was obtained from sands containing (by weight): 97.32% SiO2, 0.92% Al2O3, 0.43% Fe2O3, 0.11% TiO2, and 0.04% Cr2O3. A distinguishing feature of the technological scheme of gravity separation of sands is the counterflow motion of the initial feed and the heavy fraction.

Author
S I Evdokimov
Origin
Unknown
Journal Title
Glass And Ceramics 73 7 Nov/2016 288-292
Sector
General
Class
G 4561b

Request article (free for British Glass members)

Development Of A Technological Complex For Washing Sand
Glass And Ceramics 73 7 Nov/2016 288-292
G 4561b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.