Development In Rapid Cool Forehearths

The development of a rapid cool forehearth has enabled improvements in production rates of 20-25% to be achieved without increasing forehearth size.

Author
J Osborn, T Meade
Origin
Zedmark Refractories Ltd, Irish Glass Bottle Company Ltd
Journal Title
Glass Production Technology International 1991 119-121
Sector
Container glass
Class
C