Development Of Oxy-Fuel Technology In The Glass Industry

This paper presents an overview of information from the past, present and looks at the future of oxy-fuel technology. Authors explain the aspects of burners, refractories and furnaces and assess the rapid adoption of oxy-fuel technology for glassmaking. Also included is a selected bibliography of the many important papers written on the topic, an invaluable reference tool for more in-depth study.