Development Of Non-Lead Compositions

The development of non-lead crystalline compositions and non-lead glasses, capable of substituting lead crystal are covered in this article.

Author
L G Johansson, B Jonson
Origin
Glafo, Sweden
Journal Title
Glass Technology 34 3 1993 91-93