The Development Of Foam Glass Production

A description is given of the current production of foam glass using metal moulds and of the development of a more progressive method using continuous conveyors.

Author
J. Malesak
Origin
Unknown
Journal Title
Sklar Keram., 1971 21 (9) 232-73 (Czech)
Sector
Primary Papers
Class
PP 1023

Request article (free for British Glass members)

The Development Of Foam Glass Production
Sklar Keram., 1971 21 (9) 232-73 (Czech)
PP 1023