Development Of Float Process In Sheet Glass Production

Three independant methods for float glass production developed by Pilkington (England), PPG Industries (USA), and the saratov Institute of Glass (Russia) are described, fundamental differences between these methods are considered. Phases of the development of two-stage glass-molding technology at the saratov Institute are described.

Author
V I Kondrashov Etal
Origin
Saratov Institute Of Glass, Saratov, Russia
Journal Title
Glass And Ceramics 57 5-6 2000 195 - 199
Sector
Flat glass
Class
F 2207