Development Of Crystal Glazes

Crystalline glazes are characterised by the formation of crystals. They can be either microscopic or macroscopic, either in the glassy matrix or on the surface. The development of crystalline glazes allows us to achieve textural variations and not offer just the standard glossy or matte surfaces that are typically available. They contain materials that crystallise during the cooling period. The crystals usually occur in clusters, frequently covering considerable areas. Often, they are coloured with ceramic oxides such as copper, cobalt and nickel. The development of crystals depends on oxides, which saturate the glaze to form the corresponding silicate; the chemical and physical properties of the solvent glaze; firing and cooling conditions; and application.

Author
J Archer 7 D Schneider
Origin
Fusion Ceramics Inc, Usa
Journal Title
Cesp 25 2 2004 93-105
Sector
Enamels
Class
E 109

Request article (free for British Glass members)

Development Of Crystal Glazes
Cesp 25 2 2004 93-105
E 109
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.