Development Of A Composition Suitable For The Production Of Alkali-Resistant Glass Fibres With A Low Fibrising Temperature

The alkali resistance, liquidus temperature and viscosity of the CaO-BaO-MgO-Na2O-ZrO2-SiO2 system are measured over a range of compositions. Using regression analysis, two mixed kinds of polynomial equation are proposed from which the most suitable glass composition for the fabrication of alkali resistant glass fibres is determined.

Author
P Simurka Et Al
Origin
Glass Research And Trade Centre, Czechoslovakia
Journal Title
Glass Technology 33 4 August 1992 130-135
Sector
Glass Fibre
Class
GF 84

Request article (free for British Glass members)

Development Of A Composition Suitable For The Production Of Alkali-Resistant Glass Fibres With A Low Fibrising Temperature
Glass Technology 33 4 August 1992 130-135
GF 84
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.