Development Of Bioactive Glass - Ceramics In The System Apatite - Anorthite - Diopside

Glass-ceramics for medical needs have been synthesized on the bases of the investigation phase equilibrium in the system Ca5[PO4]F-CaAl2Si2O8-CaMgSi2O6. The formation of the main crystal phases, the structure and properties of glass-ceramics are shown.