Development And Clinical Studies Of Ha Coated Dental Implants Using Various Techniques

Titanium and titanium alloys have been popularly used as dental implant materials worldwide. On the other hand, hydroxyapatite (HA) coated titanium implants are becoming more popular, especially in Japan. Long-term good clinical results have been reported and new bone formation around the implant after implantation is fast. The authors in this paper have developed sintered HA and several HA coated implants using various coating techniques including sintering, plasma spraying, thermal decomposition, dipping, electrophoretic deposition, and sputtering.

Author
H Aoki & T Li
Origin
Saitama Inst Technol & Aoki Dental Clinic, Sichuan, China
Journal Title
J Aust Ceram Soc 47 1 2011 57-59
Sector
Glass Ceramics
Class
GC 760

Request article (free for British Glass members)

Development And Clinical Studies Of Ha Coated Dental Implants Using Various Techniques
J Aust Ceram Soc 47 1 2011 57-59
GC 760
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.