Developing The Next Generation Of Glass Enamels

For many decades glass enamles based on lead and cadmium-containing frits and stains have been widely used for the decoration of glass. Following increased concern over the risks associated with heavy metal-containing enamels used to decorate glassware, one German company has introduced a range of lead, cadmium and lithium-free enamels. This article provides an insight into how the range was developed.

Author
A Glesecke
Origin
Cerdec Ag Keramische Farben , Germany
Journal Title
Glass 75 1 1998 23-25
Sector
Enamels
Class