Determination Of The Skin Viscosity Of Glass Via Fibre Elongation

The use of fibre elongation techniques for studying the formation and resulting properties of thin, high viscosity surface layers is described.

Author
W C Lacourse & P Shen
Origin
Alfred University, Usa
Journal Title
Ceramic Trans 82 1998 341-347
Sector
Glass Fibre
Class
GF 217

Request article (free for British Glass members)

Determination Of The Skin Viscosity Of Glass Via Fibre Elongation
Ceramic Trans 82 1998 341-347
GF 217