The Determination Of Hexavalent Chromium As A Requisite To Comply With The Packaging Directive (In Italian)

EC Directive 94/62 imposes the concentration limits of heavy metals such as Pb, Cd, Hg and hexavalent chromium in packaging materials starting 30 June 1998. In the absence of a standard procedure, this paper describes a method which allows the eventual presence of hexavalent chrome to be detected and measured also in glasses with a high content in trivalent chromium, to which it is sometimes erroneously assimilated. The glass sample is decomposed in a cold mixture of H2SO4 and NH4HF2. By adding diphenylcarbazide a pink coloured comples is obtained, whose absorbance is measured at 840nm. The detection limit is 5ppm Cr03 (mg/Kg glass).

Author
E Guadagnino Et Al
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 28 2 1998 63-66
Sector
Container glass
Class
C 1189

Request article (free for British Glass members)

The Determination Of Hexavalent Chromium As A Requisite To Comply With The Packaging Directive (In Italian)
Riv Staz Sper Vetro 28 2 1998 63-66
C 1189
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.