Determination Of Different Valence Forms Of Cerium In Glasses Using Potentiometric Titration

A method has been developed to determine the total cerium concentration in glasses and to monitor the redox conditions in furnaces when melting cerium containing glasses. The method is based on titration against hydroquinone in an acid medium.

Author
S M Chesnokova, I Yu Danilova, P A Andreev
Origin
Glass And Ceramics 44 1-2 January-February 1987 31-33
Journal Title
Refer to Origin
Sector
Special Glass
Class
S 5011