Determination Of The Corrosion Progress Of Zirconium Oxide Containing Refractories Based On The Natural Intrinsic Gamma Radiation Of The Material

A measuring schedule was developed and calibrating measurements were carried out with blocks of different zirconia content. First practical tests were made on cold glass furnaces. The final adaptation of the equipment was done with measurements on operating glass furnaces.

Author
B Fleischmann Et Al
Origin
Hvg Germany
Journal Title
Glastech Ber Glass Sci Technol 74 9 2001 258-269
Sector
Refractories
Class
R 410

Request article (free for British Glass members)

Determination Of The Corrosion Progress Of Zirconium Oxide Containing Refractories Based On The Natural Intrinsic Gamma Radiation Of The Material
Glastech Ber Glass Sci Technol 74 9 2001 258-269
R 410
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.