Determinatio Of Individual Fibre Failure In Fibre Bundles

The onset of fibre failure signals the commencement of catastrophic structural failure in fibre bundle systems, a process that is important in standalone bundles and in other material structures. In this work, a technique by which the onset of fibre failure can accurately be identified by monitoring the electrical continuity and resistance of filaments and bundles during loading is demonstrated. The dual sensor/loading functionality of the fibres differs from most prior approaches wherein separate sensors were added to the load-bearing fibre array. Individual fibre failure and bundle onset failures in 50 fibre bundles were reliably and reproducibly detected.

Author
S M Toffoli & R L Lehman
Origin
University Of Sao Paulo, & Rutgers University, Usa
Journal Title
J Am Ceram Soc 84 1 2001 123-128
Sector
Glass Fibre
Class
GF 265

Request article (free for British Glass members)

Determinatio Of Individual Fibre Failure In Fibre Bundles
J Am Ceram Soc 84 1 2001 123-128
GF 265
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.