Deterioration Of Stained Medieval Glass By Atmospheric Attack Part 2. Secondary Ion Mass Spectrometry Analysis Of The Naturally Weatherd Glass Surfaces

Secondary ion mass spectrometry was applied to analyze naturally weathered medieval glass exposed to the ambient atmosphere for more than 600 years.