Detection Of Phase Separation By Ftir In A Liquid-Crystal-Display Substrate Aluminoborosilicate Glass

The effect of heat treatment on the Fourier transform infrared spectrometry (FTIR) reflection peak position of the Si-0 structural band near 1087cm-1 of a liquid-crystal-display (LCD)substrate glass was investigated. The FTIR peak position shifted more slowly with heat-treatment time, and to a greater extent than expected, for the fictive temperature change. The isochronal shirt of the FTIR peak as a function of the heat treatment temperature exhibited a good correlation with the change of chemical durability in an HCl solution, suggesting that the infrared peak shift was the result of the phase separation induced by the heat treatment.

Author
Y Kato Et Al
Origin
Rensselaer Polytechnic Inst, Usa
Journal Title
J Am Ceram Soc 84 9 2001 2111-2116
Sector
Special Glass
Class
S 2410

Request article (free for British Glass members)

Detection Of Phase Separation By Ftir In A Liquid-Crystal-Display Substrate Aluminoborosilicate Glass
J Am Ceram Soc 84 9 2001 2111-2116
S 2410
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.