Detecting Deviation On Wide Mouth Containers

The Non-Contact Planity Inspection (NCP) is a system for detecting faults in glass containers. The upper mouth edge of a container is checked by a camera system, thus ensuring that the quality demands for the sealing surface of the containers are fulfilled. It measures the entire upper mouth line (360 deg), paying particular attention to measruing level parallelism. Deviations are measured with the values of the height and perimeter or other angle. The measuring results for dip and saddle

Author
F Gunther
Origin
Optische Prufsysteme, Germany
Journal Title
Glass Worldwide 15 Jan-Feb/08 29
Sector
Container glass
Class
C 3592

Request article (free for British Glass members)

Detecting Deviation On Wide Mouth Containers
Glass Worldwide 15 Jan-Feb/08 29
C 3592
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.