Designing Of High Temperature Oil Fired Low Thermal Mass Semi-Automatic Chamber Kiln

A high temperature oil fired semi-automatic down draught chamber kiln has been designed and commissioned in the Institute. The loading volume of the kiln is 2.0 m3. The design criteria considered the reduction of thermal mass, heat loss and incorporation of a recuperation system to achieve higher fuel efficiency. The kiln is automatically operated by a microprocessor based programmable temperature controller and a PID pressure controller. The kiln is running successfully with almost 46% fuel savings with respect to conventional kilns.

Author
S Dasgupta Et Al
Origin
Central Glass & Ceramic Research Inst, Kolkata, India
Journal Title
Trans Ind Ceram Soc 60 2 April-June 2001 90-94
Sector
General
Class
G 2562

Request article (free for British Glass members)

Designing Of High Temperature Oil Fired Low Thermal Mass Semi-Automatic Chamber Kiln
Trans Ind Ceram Soc 60 2 April-June 2001 90-94
G 2562
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.