Design Multifunctional Glasses For Fast Trains And Variable Transmission Glazing For Buildings

The design of windscreen and lateral windows for fast trains has been conceived to satisfy the high level mechanical performances in addition to ballistic impact strength requested by Italian railway specifications. Furthermore optical, thermal, acoustical, solar control and luminosity of internal passenger compartment have to satisfy not only standard specifications but also new needs to be competitive in the globalisation of the products. Among the optical characteristics, the most difficult to satisfy have been the specification limits relative to the difference in colour transmission and haze, both concerning the windscreen, which has to be heatable by alternative technologies, including direct coating or conductive polymer films in order to achieve de-icing performance. One solution here looks at a composite glass-polycarbonate laminate glazing.

Author
G Manfre
Origin
Isoclima Spa, Italy
Journal Title
Proc Xvii Icg Vol 5 Beijing 1995 43-48
Sector
Flat glass
Class
F 1204

Request article (free for British Glass members)

Design Multifunctional Glasses For Fast Trains And Variable Transmission Glazing For Buildings
Proc Xvii Icg Vol 5 Beijing 1995 43-48
F 1204
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.